I have a springfield 45 in stainless whats a good polish for removing scratches and shining it up a bit.any sugggestions on products or methods appreciated
__________________
TRESPASSERS WILL BE SHOT AND SURVIVORS WILL BE SHOT AGAIN
dragonfire is offline  
Old March 29, 2006, 01:17 AM   #2
Dfariswheel
Senior Member
 
Join Date: May 4, 2001
Posts: 7,478
To remove scratches, use Scotchbrite pads.
These are synthetic "sanding and polishing" pads sold in automotive stores for use during painting a car.

Select one that most closely matches the guns original grained finish and rub the scratches until they're gone, or at least blended in with the rest of the gun.

To finish off, "stroke" the pad in the same direction the original grain runs.

To shine up, use any good stainless polish, like Mother's Mag polish, MAAS, Flitz, or any other.

Do not use the pads or the polish on the areas of the gun that have a bead blasted finish, like the top of the frame.
The only way to re-do those areas is by re-bead blasting them.

DO NOT use steel wool on a stainless gun to remove scratches.
The steel wool will embed tiny particles into the stainless.
Later the mild steel particles will rust, damaging the stainless.
Dfariswheel is offline  
Old March 29, 2006, 12:41 PM   #3
Unclenick
Staff
 
Join Date: March 4, 2005
Location: Ohio
Posts: 21,060
If your automotive store doesn't carry them all, go to one of the industrial supply sites and you will find the Scotchbrite abrasive in grades all the way down to a polish. Try MSC, but there are others, as well.

If you have to remove a scratch close to where bead blasting starts (top edge of the side of the slide, for example) consider using wet/dry paper that has been put on a flat surface with a spray adhesive and pull the slide along it. Again, you can go through grades. It would take a lot of this to get a serious scratch out, and the pads are better for that. Assuming you don't own a granite surface plate, the flat surface can be a piece of tempered plate glass. Gluing several layers of plate glass together to make a surface plate is an old technique. Use an epoxy for bonding them.

Nick
__________________
Gunsite Orange Hat Family Member
CMP Certified GSM Master Instructor
NRA Certified Rifle Instructor
NRA Benefactor Member and Golden Eagle
Unclenick is offline  
Old March 31, 2006, 11:00 AM   #4
Harry Bonar
Senior Member
 
Join Date: December 5, 2004
Location: In the Vincent, Ohio general area.
Posts: 1,804
polish stainless

Dear Sir:
I simply love beadblasting with fine beads - it looks great and if you scratch it just bead it lightly again!
Harry B.
Harry Bonar is offline  
Reply

Thread Tools Search this Thread
Search this Thread:

Advanced Search

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -5. The time now is 03:56 PM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2024, vBulletin Solutions, Inc.
This site and contents, including all posts, Copyright © 1998-2021 S.W.A.T. Magazine
Copyright Complaints: Please direct DMCA Takedown Notices to the registered agent: thefiringline.com
Page generated in 0.03998 seconds with 10 queries