OneQuikSix - quick & honest!
Chris made me a deal I couldn't refuse.
Used everything today: 1. Lee electric casting furnace (10lb capacity) 2. Lee aluminum 6 cavity bullet mold for 40 S&W/10mm 175grn 3. Lyman 1lb ingot mold It worked perfect. All deals should go this smooth. Thank you, Sir! George |
May 3, 2008, 09:43 PM | #2 |
Junior member
Join Date: September 26, 2007
Posts: 1,919
|
Which Chris?
|
May 3, 2008, 09:45 PM | #3 |
Junior member
Join Date: April 15, 2008
Location: Ohio - lower left hand corner
Posts: 84
|
Hey Doc... quit bustin on me!
OneQuikSix. It is in the title. |
May 3, 2008, 09:50 PM | #4 |
Junior member
Join Date: September 26, 2007
Posts: 1,919
|
DUH! Now i feel stupid......
|
May 3, 2008, 09:54 PM | #5 |
Junior member
Join Date: April 15, 2008
Location: Ohio - lower left hand corner
Posts: 84
|
Ha, ha.
It's all good my fellow Proud American! |
May 6, 2008, 06:47 AM | #6 |
Junior Member
Join Date: November 19, 2007
Location: Georgia
Posts: 14
|
Glad everything worked out for you...hope you have many years of good service out of everything you bought.
|