Savage model 24 solder
Will the solder used on the barrels of early model 24's hold up in the hot blueing tank temperatures bringing used today?
|
April 18, 2018, 09:42 PM | #2 |
Senior Member
Join Date: June 24, 2008
Posts: 2,607
|
Probably not.
__________________
Time Travelers' Wisdom: Never Do Yesterday What Should Be Done Tomorrow. If At Last You Do Succeed, Never Try Again. |
April 19, 2018, 12:48 PM | #3 |
Senior Member
Join Date: February 13, 2002
Location: Canada
Posts: 12,453
|
Blueing tank temperatures are no different now than they were 100 years ago. 275 °F to 310 °F (135 °C to 154 °C).
If the Savage 24 barrel is even connected over its whole length, you want "Rust Bluing".
__________________
Spelling and grammar count! |
April 19, 2018, 12:50 PM | #4 |
Senior Member
Join Date: October 25, 2001
Location: Alabama
Posts: 18,541
|
It's not the temperature, it's the chemistry. Hot bluing salts contain a lot of sodium hydroxide (lye, caustic soda). It has no effect on the steel, its purpose is to raise the boiling point of the solution to where the nitrates will work.
Hot lye will dissolve soft (lead based) solder. Don't do it. |
|
|