Sorry Snuffy, I should have stated the material. The .44 is a Lee aluminum two holer (429-200-RF) . I smoked the mold after reading the reviews at the Midway site where I bought the mold. Since I am new to casting I just assumed that since they all raved about how deeply they smoked the molds that it was necessary!
I'll check for the burrs but I had no problem with sticking at all for the first 100 or so castings. Then they started sticking one out of each casting then BOTH started sticking each time. I figured it was time to stop casting and get some advice.
It just occurred to me that maybe the problem was more to do with something in the melting pot that was building up with time? I was fluxing when I noticed any buildup on the surface of the melt.