Trouble with aluminum molds (sticking)
I am new to aluminum molds (Lee), so far I can say I much prefer the steel Lyman molds, of which I have many, and no problem operating them.
I am having trouble with the bullets sticking in these Lee molds, I have adjusted the casting temp all over, I have been re-smoking the mold every 10-12 castings, this is the only thing that has been effective. bullets come out in good quality, they just get hard to remove after about 10 castings.
I am considering trying one of the various mold release products, or just spending some money on new Lyman molds.
Anyone have any idea what I am doing wrong?