I did hot salt bluing for about 20 years with a set-up and chemicals sold by Heatbath Corporation. The chemical was a Nickel Pentrate salt and actually penetrated the steel about .0005"+ (1/2 a thousanth +). It was not a built up coating on the steel and did not change sizes or dimensions. It was a very durable and lasting finish.

4/0 steel wool will most definitely remove factory bluing.