Tonight was my first time I've casted since college (almost 2 decades). Beeswax was used to flux the lead (from wheelweights) and a short while after fluxing, stirring, scimming and casting a few bullets, a new layer of scum would form on the surface. I found myself repeatedly scimming (and sometimes fluxing & stirring). Is this normal?