Glass bead gives a nice satin finish, shot peening gives a relatively smooth finish, sand blasting gives a very matte finish. For 1911 slides, I like either sand blasting or graining with 150 or 180 grit. Originally, the matting on 1911 slides and frames was done with wire wheels at the factory.