I think I misunderstood the question, though. I thought we were talking about glass bedding a rifle in the factory stock. If so, then yes, 2 weeks. If you meant how long to turn a complete restocking (inlet, shape, sand, and finish a semi-finished precarved stock), it's about 2 months from the time I get the stock (about 1 month of that is just applying finish letting the finish cure). If you want checkering, double that (I do checkering in batches).