That is strange. I use Tempilaq 450, 700, and 750. I have noticed that if it isn't thinned properly that it won't melt properly...but if you have used it before, I'm sure you don't put it in clumpy.

I suppose your Tempilaq 800 could be too thin or your 750 too thick.

Oh, an I also assume you are putting it on clean brass, same caliber, same headstamp, same lot etc..

But beyond that I have no idea.