The first pour into a cast-iron ingot mold (for equivalent), will cool rapidly and dump easily almost as soon as if "freezes". However, it you are pouring a lot of lead, the as the mold gets hot and stays hot, the ingots will begin to stick until they get cooler...even cast iron molds.