View Single Post
Old January 7, 2014, 04:25 AM   #6
oldandslow
Senior Member
 
Join Date: October 2, 2007
Posts: 641
bc, 1/7/14

I've done about 7,000 cases over the last year and a half and have not run into any trouble with my cases. I usually resize and deprime before stainless steel tumbling however. I've done .45acp, 44sp, 9mm, 38sp, .357 mag, .223/556, 30-30 and 30-06 withoug problems. I resize and reload on several different machines including the Dillon Square Deal B, RCBS rockchucker and Dillon 650. My ss pin tumbling recipe is one-half tablespoon laundry soap (usually Gain), one-half tablespoon dishwashing soap (whatever brand is on sale) and two tablespoons of vinegar (lemon juice works too). I tumble them for anywhere from four hours to twenty-four hours. I'm not sure why you're having problems with your setup but hope it all works out well.

best wishes- oldandslow