Old Roper...do you find the nosler 280 AI brass is the way to go? Opposed to fireforming 280 rem brass? Its less work, thats for sure! The last batch of Nosler cusrom brass I got for a different rifle I was pretty disappointed in it. Way over trimmed the case length and the contricity on the neck from case to case was not good. But they're the only ones I know of that are making AI brass. The barnes guys told me to start at a max load from their 280 rem data and work up to about 7-10% above that...do you think that would be a general rule to start with?