Corrosive primers contain the following chemicals: Potassium Chlorate, Antimony Sulfide, Lead Sulfocyanate and a small percentage of TNT.

The Chlorate salts are the ones that absorb water from the air and cause rusting.

The soap and water clean up is the best way to get rid of the salts left over from firing.