I think you'll find that the "stick" formulation you first mentioned sets up way too fast to be of any use in rifle bedding. I've used some for various mechanical repairs around the place and when it reaches a nice even color--per directions--you've only got a couple of minutes to get everything in place before the reaction "kicks over" and it starts to harden. In my shop I use Acraglas Gel and have no complaints. Goat