I used acetone with 0000 steel wool then Formby's Tung Oil which is really a varnish. I sand with 0000 steel wool, blow the dust off with an air compressor and apply 6 to 8 coats. I sand between each coat with 0000 steel wool. I like High Gloss but also comes in semi gloss and satin. Excellent product. Tim