Sounds great! I've found that a mould has a temp it prefers and there is an optimum temp for the alloy as well. Only problem is that these preferences vary from mould to mould. When I get wrinkled bullets I just cast faster until they smooth out; I'll preheat the moulds but once I get them close I let the alloy finish heating them up.