I use an acid brush and paint the area

I use an acid brush and paint the area that needs filling in Remember your release compound.
A skim bed is where I need to remove 1/8 inch and re-bed. The skim bed is for glass jobs that are old.
I coat the metal and stock in the areas with vasoline.