Doc,

I've never used hat felt; but, with the pre-punched DuroFelt wads, its quite easy to tell if each wad is fully lubricated by visual inspection. After doing it for a while, you get a feel how mush lube shavings are need to do up a tin of wads. Previously, I didn't mention that the wads are set flat, evenly distributed in the tin, so it's the same number of wads and measure of lube each time. The finished wads are very uniform.