If it don't melt, don't forceit! LOL! As stated above, those are WW's that need to be culled. Zinc melts at 781*-ish, while lead melts at over 100 degrees cooler. So, once you lead WWs start to melt, get ready to flux before scraping your clips and non-lead ww's out of the mix. You do not want to melt the zinc ww's in your melt. It ruins the castability of the lead. good luck!