Take a lesson from the father in laws oversight and when you cast your ingots take a few minutes with a scratch awl and lable the ingots with quick refference like PB for lead, WW for wheel weights, L for lino type, L#2 for Lyman #2 , 20/1 PB/SN ( lead to tin ) etc. etc. . I have moulded several small lots of different alloys over time and without doing this you end up half crazy trying to remember which ones are which. When in doubt I just make sinkers ,,,