well the tempilstic turned out to be a [color=#FF0000]█[/color][color=#FF0000]█[/color][color=#FF0000]█[/color][color=#FF0000]█[/color], I hate wasting money:barf:. I should have thought of that when the desrciption of the thing says temp. indicating "crayon" this thing is no where near a crayon it more like chalk. when I try to mark with it it just crumbles and leaves nothing on the case. maybe I got a bad one but it works for someone cause I read where on the 6mmbr on how to anneal brass webpage they use tempilstics. maybe ill think of something but I got nothin now, anybody got any suggestions with the tempilstic?