I use one for my rifle brass before, and after FL resizing. Though I have the small HF one pint. It goes for 3 mins at a time. It usualy takes about 3 cycles for not too awful dirty brass, 4 or 5 for fairly dirty. Super cruddy stuff goes on the tumbler, as well as dirty bucket handgun brass.