Cast another 250 or so TL bullets this morning. Quit @ 10a, already 93 degrees.
Put a few ounces if tin in the melt and fill improved dramatically. This bunch of WW has a slight tin deficiency. Two cavity Lee mould so much faster than my single cavity Lyman rifle moulds but I fould myself thinking about a six-cavity mould for my 45ACP casting. My two cavity mould is difficult to get lined up right every time and I'm thinking I might as well upgrade if I'm going to replace it.