MP-Mold 125gr .359 HP for 9mm

I just ordered one of these this morning. The only mold I have used is a Lee mold for 9mm .356 round nose 124gr tumble lube. It works OK.

The MP-Mold will have one grease groove instead of the many shallow grooves the Lee mold has. Can I still tumble the bullets in LLA? I'm thinking that won't be enough lube.

I have read brief mentions of pan lubing. From what I gather, you put some solid stick lube in a pan and melt it for your bullets, but haven't found anything telling me whether I just do a tumble in the melted lube then drain or what?

I am leaning towards getting the RCBS Lubrisizer and die.

What advice do you people have?