Guess I'll try casting some 40's with the ww only and try water quenching to see what I get. I can use the antimony and tin to alloy about 100# of pure lead I've got if I don't need it for the ww's. I've heard a thousand different opinions on percentages. The last batch I did was 90/5/5, but I've read that much tin and antimony may not be necessary? Hate to waste the expensive stuff!