Quote:
The alloy was pure lead, chilled shot and tin solder
I suspect it is the chilled shot. I've found this in some lead I've mixed in the past with using shot.
__________________
My posts are things I have tried or experienced. You may or may not wish to emulate them so read them with this in mind.