Quote:
I use 2.5 or 3 ounce stainless steel "condiment cups" for ingot molds. The ingots weight about 1.5 pounds each -- more when I cast soft lead. And the ingots knock right out.
I completely forgot about those. They do work well. I don't use them because the ingots are hard to stack for storage.