Pumpblast,
Use the range salvage as is. I always melt mine into ingots to clean them up so no dirt or moisture gets into the melting pot. If you're concerned about hardness, mix range salvage half and half with wheel weights. About the only time hardness is really a factor is if you're gonna run some hot loads.

------------------
johnnyb
A slow hit beats a fast miss.